MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® XFR 6842 GF10 PBT, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Celanex XFR 6842 GF10 is a halogen and antimony free flame retardant (V-0 @ 0.4 mm) 10% glass reinforced PBT grade with good processability and no corrosive emissions during processing. It is suitable for parts requiring enhanced tracking resistance, tou

Information provided by Celanese Corporation.

Key Words: Halogen Free, 10% glass filled, flame retardant PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm0.011 - 0.013 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm0.010 - 0.012 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8181ISO 2039-2
Tensile Strength at Break 70.0 MPa10200 psi5mm/min; ISO 527-2/1A
Elongation at Break 3.4 %3.4 %5mm/min; ISO 527-2/1A
Tensile Modulus 5.10 GPa740 ksi1mm/min; ISO 527-2/1A
Izod Impact, Notched (ISO) 4.50 kJ/m²2.14 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.420 J/cm²2.00 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+14 ohm-cm3.00e+14 ohm-cmIEC 60093
Surface Resistance 3.00e+15 ohm3.00e+15 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 450 V450 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 173 °C343 °FISO 75-1, -2
Vicat Softening Point 205 °C401 °FB50 (50°C/h 50N); ISO 306
Flammability, UL94 V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 
Descriptive Properties
Melt volume rate (MVR), cm³/10min12
MVR test load, kg2.16
MVR test temperature, °C250

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beijing Ranger Chem PBT 403 M-G15 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Celanese Celanex® XFR 6842 GF15 PBT, 30% Glass Reinforced
Celanese Celanex® XFR 6842 GF30 PBT, 30% Glass Reinforced
Mitsubishi Novaduran® 5010N6-3X Polybutylene Terephthalate
Mitsubishi Novaduran® SEF-500T Polybutylene Terephthalate

PHCS107 / 123522

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.