Celanese Celcon® M140-L1 POM, Tribological
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
Material Notes:
Celcon« M140-L1 is a general purpose acetal copolymer material with a slightly lower viscosity for improved flow in molding that has been modified to reduce or eliminate noise (squeak) when wearing against itself.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.40
g/cc
0.0506
lb/in³
ISO 1183
Density of Compound
1.165
g/cc
0.04209
lb/in³
Linear Mold Shrinkage, Flow
0.019
cm/cm
0.019
in/in
ISO 294-4
Linear Mold Shrinkage, Transverse
0.017
cm/cm
0.017
in/in
ISO 294-4
Melt Flow
12
g/10 min
@Load 2.16 kg,
Temperature 190 °C
12
g/10 min
@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
63.0
MPa
9140
psi
50mm/min; ISO 527-2/1A
Elongation at Yield
9.5 %
9.5 %
50mm/min; ISO 527-2/1A
Tensile Modulus
2.60
GPa
377
ksi
50mm/min; ISO 527-2/1A
Flexural Modulus
2.50
GPa
363
ksi
ISO 178
Izod Impact, Notched (ISO)
5.70
kJ/m²
2.71
ft-lb/in²
ISO 180/1A
Charpy Impact, Notched
0.600
J/cm²
2.86
ft-lb/in²
ISO 179/1eA
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
110
µm/m-°C
61.1
µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow
120
µm/m-°C
66.7
µin/in-°F
ISO 11359-2
Melting Point
166
°C
331
°F
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi)
100
°C
212
°F
ISO 75-1, -2
Processing Properties
Metric
English
Comments
Processing Temperature
80.0
-
120
°C
176
-
248
°F
cavity
180
-
200
°C
356
-
392
°F
hot runner
Zone 1
170
-
180
°C
338
-
356
°F
Zone 2
180
-
190
°C
356
-
374
°F
Zone 3
180
-
190
°C
356
-
374
°F
Zone 4
190
-
200
°C
374
-
392
°F
Die Temperature
190
-
200
°C
374
-
392
°F
Melt Temperature
180
-
200
°C
356
-
392
°F
Drying Temperature
80.0
-
100
°C
176
-
212
°F
Dry Time
3.00
hour
3.00
hour
Injection Pressure
60.0
-
120
MPa
8700
-
17400
psi
Hold Pressure
60.0
-
120
MPa
8700
-
17400
psi
Back Pressure
<=
4.00
MPa
<=
580
psi
Descriptive Properties
Injection molding
Yes
Injection speed
slow-medium
Pellets
Yes
Processing conditions acc. ISO
9988-2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Celcon® LW90-F2 POM, Tribological
Celanese Celcon® LW90-S2 POM, Tribological
Celanese Celcon® LW25-S2 POM, Tribological
Celanese Hostaform® LW90EWX POM, Tribological
Celanese Celcon® GB10 POM, 10% Glass Reinforced
PHCQ116 / 178571
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.