MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI LAESTRA E01 G/30 30% Glass Fiber Reinforced, Elastomer Modified Syndiotactic Polystyrene (SPS)  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Syndiotactic Polystyrene (SPS); Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber

Material Notes: Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270°C and a glass transition temperature of 100°C, therefore it is an alternative to more expensive high temperature materials. Laestra compounds retain excellent property performance levels and dimensional stability at high temperature environments/applications like under the hood components or IR soldering of connectors. Laestra provides a resistance against a wide range of acids, bases and organic solvents. Moreover, it does not absorb moisture and is not affected by water at room or high temperatures. Glass Reinforced Laestra offers high rigidity at high temperatures and lower differential shrinkage compared to other semi-crystalline resins. However the presence of glass fiber still requires an accurate design in order to reduce the risk of warpage.

Specific Notes for this Material: SPS, 30% glass fiber, elastomer modified

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inLATI
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 110 MPa16000 psiISO 527
Flexural Modulus 8.10 GPa1170 ksiASTM D790
Izod Impact, Notched 1.05 J/cm
@Temperature 23.0 °C
1.97 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 17.0 kV/mm
@Thickness 2.00 mm
432 kV/in
@Thickness 0.0787 in
IEC 243-1
Comparative Tracking Index >= 400 V>= 400 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 225 °C437 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 - 325 °C572 - 617 °F
Mold Temperature 100 - 150 °C212 - 302 °F
Drying Temperature 80.0 - 100 °C176 - 212 °FNot essential. Moisture pickup may occur under adverse, high humidity conditions.
Dry Time >= 2 hour>= 2 hour
 
Descriptive Properties
Injection Speedhigh

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Idemitsu Kosan Xarec® EA 513 SPS, 30% Glass Filled
Dow Questra® EA503 High Heat Syndiotactic Polystyrene, 30% Glass Filled
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance
Dow Questra® WA551 High Heat Syndiotactic Polystyrene, 40% Glass Filled
INEOS Styrolution PS 1611 GPPS

PLATI223 / 50221

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.