MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled; Polyethylene Terephthalate (PET)

Material Notes: PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stability

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.74 g/cc1.74 g/ccISO 1183
Bulk Density 1.00 g/cc0.0361 lb/in³ISO 60
Viscosity Number 50 cm³/g0.50 dl/gISO 1628-5
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.0020 cm/cm0.0020 in/in60x60x2; 280°C / WZ 110°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0020 cm/cm0.0020 in/inPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.0070 cm/cm0.0070 in/in60x60x2; 280°C / WZ 110°C; 600 bar; ISO 294-4
Melt Flow 21 g/10 min
@Load 2.16 kg,
Temperature 280 °C
21 g/10 min
@Load 4.76 lb,
Temperature 536 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psiISO 527-1, -2; 5 mm/min
Elongation at Break 1.3 %1.3 %ISO 527-1, -2; 5 mm/min
Tensile Modulus 12.7 GPa1840 ksiISO 527-1, -2; 1 mm/min
Flexural Strength 170 MPa
@Strain 1.7 %
24700 psi
@Strain 1.7 %
2 mm/min; ISO 178-A
Flexural Modulus 12.8 GPa1860 ksi2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  25.0 kJ/m²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
 25.0 kJ/m²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
Charpy Impact Unnotched  2.50 J/cm²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
 <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+20 ohm-cm2.00e+20 ohm-cmIEC 60093
Surface Resistance 5.40e+16 ohm5.40e+16 ohmIEC 60093
Dielectric Constant  4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
IEC 60250
 4.3
@Frequency 100 Hz
4.3
@Frequency 100 Hz
IEC 60250
Dielectric Strength 33.0 kV/mm
@Thickness 1.00 mm
838 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0022
@Frequency 100 Hz
0.0022
@Frequency 100 Hz
IEC 60250
 0.0138
@Frequency 1e+6 Hz
0.0138
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 275 V275 Vd.a.m.; Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1, -2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FISO 8302
Melting Point 255 °C491 °F10°C/min; ISO 11357-1, -3
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1, -2
Vicat Softening Point 225 °C
@Load 5.10 kg
437 °F
@Load 11.2 lb
120°C/hour; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °F
 280 °C536 °Ffor test specimens; ISO 294
Mold Temperature 110 °C230 °Ffor test specimens; ISO 294
 100 - 130 °C212 - 266 °F
Drying Temperature 120 °C248 °F
Dry Time 4 - 8 hour4 - 8 hour
Moisture Content 0.00 - 0.020 %0.00 - 0.020 %residual; Karl Fischer Test
 
Descriptive Properties
ISO Short NameISO 7792-1-PET+PBT, GHMR, 07-120, (GF+MD)44

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BCF 30 X H2.0 901510 Nylon 6 (PA6), 30% Glass/Carbon Fiber Reinforced, Dry
Evonik Vestodur® X7085 45% Glass Fiber Reinforced PBT
Mitsubishi Reny® 1012H Polyamide
Mitsubishi Reny® 2041 Polyamide
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced

PLANX0672 / 133635

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.