MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LGflex BET Plasticizer  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: LGflex BET is the new material developed by LG for the time in the world. Certified as a product that conforms to the standards of 21 CFR (FDA) and 16 CFR (Acute Oral Toxicity) of the code of federal regulations in the US. LGflex BET is an environment-friendly (non-endocrine disrupter) plasticizer for PVC soft sheet and injection, with excellent volatile resistance, migration resistance and improved odor qualities.

Application: Non-toxic Sheets, Toys, Interior and External Decoration of Automobiles

CSA No. 610787-76-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 490 g/mol490 g/mol
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10
@Treatment Temp. 125 °C,
Time 10800 sec
<= 0.10
@Treatment Temp. 257 °F,
Time 3.00 hour
After Heating, KOH mg/g; JIS K6751
 
Thermal PropertiesMetricEnglishComments
Melting Point -41.0 °C-41.8 °FFreezing Point
Boiling Point 346 °C
@Pressure 0.101 MPa
655 °F
@Pressure 14.7 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Acidity<0.1 KOH mg/gJIS K6751
Color<150 APHAJIS K6751

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LGflex GL300 Plasticizer
LG Chemical LGflex GL100 Plasticizer
LG Chemical LGflex EBNW Plasticizer
LG Chemical DOP Plasticizer
LG Chemical DOA Plasticizer

PLAY251 / 148261

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.