DENSIL DF Antimicrobial is a broad-spectrum fungicide/algaecide for the dry film protection of aqueous based surface coatings. DENSIL DF Antimicrobial is an aqueous dispersion of methyl-N-(2-benzimidazolyl) carbamate, N’-3,4-dichlorophenyl)-N,N-dimethylurea and 2-N-octyl-4-isothiazolin-3-one. Applications The product is particularly effective as a single active dry film preservative for Architectural & Industrial Paints & Coatings. Antimicrobial Properties The levels of DENSIL DF Antimicrobial needed to prevent the growth of problem micro-organisms are listed in Table 1. MIC’s do not represent effective use levels but do indicate the broad spectrum of activity of DENSIL DF Antimicrobial.Information provided by Excel Industries Ltd. |