MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Radici Radilon® A CF350 (dry) Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.

Information provided by Radici group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/cc
Water Absorption 5.6 %5.6 %
Moisture Absorption at Equilibrium 1.3 %1.3 %
Viscosity Number 270 cm³/g2.70 dl/g
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 230 MPa33400 psi
Elongation at Break 1.5 %1.5 %
Tensile Modulus 28.2 GPa4090 ksi
Charpy Impact Unnotched  4.10 J/cm²
@Temperature -30.0 °C
19.5 ft-lb/in²
@Temperature -22.0 °F
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched  0.490 J/cm²
@Temperature -30.0 °C
2.33 ft-lb/in²
@Temperature -22.0 °F
 0.660 J/cm²
@Temperature 23.0 °C
3.14 ft-lb/in²
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm1000 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F
Deflection Temperature at 0.46 MPa (66 psi) 245 °C473 °F
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °F
Vicat Softening Point 240 °C
@Load 5.10 kg
464 °F
@Load 11.2 lb
50°C/h
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Radici Radilon® SRV300 (dry) Nylon 6
Radici Radilon® A RV500 (dry) Nylon 66
Radici Radilon® A CP400 (dry) Nylon 66
Akro-Plastic Akromid® C3 GF 60 1 black (4353) PA66 + PA6, Conditioned, 60% Glass Filled
Techmer ES HiFill® PA6 CF40 40% Carbon Fiber Filled

PRADI807 / 120320

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.