MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sichuan Deyang Haton® hb DL Polyphenylene Sulfide Resin
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Extrusion, low chlorine

Information provided by Sichuan Deyang Chemical Co., LTD

Key Words: UL E236625
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption <= 0.50 %<= 0.50 %GB/T 2914-2008
Molecular Weight >= 40000 g/mol>= 40000 g/mol
Melt Flow 800 g/10 min800 g/10 minGB/T 3682-2000
Ash <= 2.5 %<= 2.5 %GB/T 9345.1-2008
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 50.0 MPa>= 7250 psiGB/T 1040.2-2006
Elongation at Break >= 2.1 %>= 2.1 %GB/T 1040.2-2006
Flexural Strength >= 110 MPa>= 16000 psiGB/T 9341-2008
Flexural Modulus >= 3.00 GPa>= 435 ksiGB/T 9341-2008
Izod Impact, Unnotched (ISO) >= 3.00 kJ/m²>= 1.43 ft-lb/in²GB/T 1843-2008
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °FGB/T 16582-2008
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® XP-4240 PPS/PPA
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material
Shakespeare HPA-40 diameter 0.5 mm PPS Monofilament
Sichuan Deyang Haton® hb Polyphenylene Sulfide Resin
Sichuan Deyang Haton® hd Polyphenylene Sulfide Resin

PSICHU939 / 156180

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.