MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2700 S-60A UV Saturated Styrenic Block Copolymer UV Stabilized
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/ccASTM D 792
Linear Mold Shrinkage 0.020 - 0.030 cm/cm
@Thickness 3.20 mm
0.020 - 0.030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 616110 s delay; ASTM D 2240
Tensile Strength at Break 5.085 MPa737.5 psiASTM D 638
 8.832 MPa1281 psiASTM D 412
100% Modulus 1.81 MPa
@Strain 100 %
262 psi
@Strain 100 %
ASTM D 412
Tear Strength 33.5 kN/m191 pliDie C; ASTM D 624
Peel Strength 4.56 kN/m26.0 pliPP (50% VLF); Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
 >= 6.14 kN/m>= 35.0 pliPP (30% VLF); Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
 >= 6.14 kN/m>= 35.0 pliPP; Failure Type R; 90 degrees, 20 in/min (500 mm/min); ISO 813
Compression Set  21 %
@Temperature 23.0 °C,
Time 79200 sec
21 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 46 %
@Temperature 70.0 °C,
Time 79200 sec
46 %
@Temperature 158 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 163 - 204 °C325 - 400 °F
Mold Temperature 15.6 - 37.8 °C60.0 - 100 °F
Drying Temperature 76.7 °C
@Time 7200 - 14400 sec
170 °F
@Time 2.00 - 4.00 hour
Moisture Content 0.040 %0.040 %
Injection Pressure 34.5 - 68.9 MPa5000 - 10000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 6091 B-60A BLACK Specialty Thermoplastic Elastomer, PA-6 bondable - manufactured with Santoprene™ TPV technology
RTP Company RTP 6003-75A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
RTP Company RTP 2740U-90A  Saturated Styrenic Elastomer (SBS) 90 Shore A
RTP Company RTP 2740 S-45A Saturated Styrenic Block Copolymer (TES/SEBS or other)
RTP Company RTP 2700 S-30A HB Saturated Styrenic Block Copolymer; General Purpose

PQZWA990 / 92530

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.