MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman ComAlloy Lubrilon® 629 Nylon 6/6, Glass Fiber/PTFE Filled, Flow Enhanced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber/PTFE Filled

Material Notes: Data provided by the manufacturer, ComAlloy International Company.

High performance and excellent lubricity with minimal surface wear.

The ComAlloy product line has been integrated into the A Schulman product line.

Key Words: Polyamide 6/6; Polyamide 66; Nylon 66; ComAlloy International Company, subsidiary of A. Shulman Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 117117ASTM D785
Tensile Strength, Ultimate 163 MPa23600 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Flexural Strength 214 MPa31000 psiASTM D790
Flexural Modulus 9.40 GPa1360 ksiASTM D790
Izod Impact, Notched 0.960 J/cm1.80 ft-lb/inASTM D256
Izod Impact, Unnotched 6.94 J/cm13.0 ft-lb/inASTM D256
K (wear) Factor 28.2 x 10-8 mm³/N-M14.0 x 10-10 in³-min/ft-lb-hrK=W/PVT where W=wear (inches^3); P=applied pressure (psi); V=velocity (fpm); T=time (hours).
Limiting Pressure Velocity 0.700 MPa-m/sec20000 psi-ft/min
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 - 275 °C491 - 527 °F
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 249 °C480 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 271 - 285 °C520 - 545 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
Chase Plastics CP Pryme® NN130GMD2HS (DAM) Nylon 66, 30% Glass Fiber Reinforced, 2% MoS2 Lubricated, Heat Stabilized
Eurotec® Tecomid® NA40 GR30 NL RT PA6.6, 30% glass fiber reinforced, PTFE modified, natural
E-Polymers TEKAMID® TA210 LW TA210LW, Low Wear, Low Friction PA66, DAM
Evonik Trogamid® A4000 Transparent Polyamide

PASH1H / 24816

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.