MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound; Filled/Reinforced Thermoset

Material Notes: High flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over molding.

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 g/cc0.0181 lb/in³ISO 60
Density 1.80 g/cc0.0650 lb/in³ISO 1183
Water Absorption 0.060 %0.060 %ISO 62
Linear Mold Shrinkage 0.0014 cm/cm0.0014 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 96.0 MPa13900 psiISO 527-1
Elongation at Break 0.60 %0.60 %ISO 527-1
Tensile Modulus 17.0 GPa2470 ksiISO 527-1
Flexural Strength 204 MPa29600 psiISO 178
Flexural Modulus 15.0 GPa2180 ksiISO 178
Compressive Strength 232 MPa33600 psiISO 604
Charpy Impact, Notched 4.60 J/cm²21.9 ft-lb/in²ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 28.0 kV/mm711 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 5.70 µm/m-°C3.17 µin/in-°FTMA
CTE, linear, Transverse to Flow 69.0 µm/m-°C38.3 µin/in-°FTMA
Glass Transition Temp, Tg 165 °C329 °F
 
Descriptive Properties
ColorDark Grey
Molding MethodCompression
 Injection
 Transfer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
Sumitomo Bakelite NEONIT® SK60 L8F Epoxy Molding Compound
Vyncolit Neopreg Kinel® SK60 L8F Glass Fiber Reinforced Molding Compound
Norplex-Micarta StatNot MC511SN Epoxy Glass Laminate Sheet
Norplex-Micarta RT500F Epoxy Fiber Glass Laminate Tube, NEMA G-10

PVYNCN940 / 142715

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.