MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker HDK® T30P Silica
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Synthetic, hydrophilic, amorphous silica, produced via flame hydrolysis. Standard product for industrial applications.

Special features: White colloidal powder of high purity.

Application: HDK® T30P is used as a reinforcing filler in elastomers, mainly silicone-elastomers

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.100 g/cc0.00361 lb/in³tamped; DIN EN ISO 787-11
Density 2.20 g/cc0.0795 lb/in³DIN 51757
pH 3.8 - 4.33.8 - 4.34% dispersion; DIN EN ISO 787-9
Specific Surface Area 270 - 330 m²/g270 - 330 m²/gHydrophobic Silica
Evaporation Loss <= 1.5 %
@Temperature 105 °C,
Time 7200 sec
<= 1.5 %
@Temperature 221 °F,
Time 2.00 hour
DIN EN ISO 787-2
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.461.46
 
Component Elements PropertiesMetricEnglishComments
SiO2 >= 99.8 %>= 99.8 %based on the substance heated at 1000°C for 2 h; DIN EN ISO 3262-19
 
Descriptive Properties
Sieve residue<0.03%acc to Mocker >40 µm, DIN EN ISO 787-18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Dioxide, SiO2 (Beta Cristobalite)
Wacker HDK® H20 Silica
Wacker HDK® N20 Silica
Silicon Dioxide, SiO2 (Coesite)
Morgan Advanced Ceramics HVX Silica

PWACK9355 / 204884

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.