MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grivory® GTR 45 PA6I/6T
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides the most interesting property of Grivory GTR 45 is the transparency even at high wall thicknesses. Grivory GTR 45 is suitable for production of optically and technically demanding parts in the application segments:
  • Electro / Electronics
  • Mechanical engineering
  • Domestic appliances
  • Safety technology
  • Packaging
Grivory GTR 45 can be used where transparency with solvent resistance is needed and is particularly suitable and approved for parts in contact with non alcoholic food, cosmetics and cold ( < 30°C) drinking water.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³Dry; ISO 1183
Water Absorption 7.0 %7.0 %Sim. to ISO 62
Moisture Absorption 2.00 %2.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 145 MPa21000 psiDry; ISO 2039-1
 145 MPa21000 psiConditioned; ISO 2039-1
Tensile Strength, Yield 100 MPa14500 psiDry; ISO 527-1/-2
 100 MPa14500 psiConditioned; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal, Dry; ISO 527-1/-2
 >= 50 %>= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %Dry; ISO 527-1/-2
 5.0 %5.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 3.00 GPa435 ksiDry; ISO 527-1/-2
 3.00 GPa435 ksiConditioned; ISO 527-1/-2
Charpy Impact, Notched  0.200 J/cm²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cm1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 27.0 kV/mm686 kV/inDry; IEC 60243-1
 27.0 kV/mm686 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-1/-2
Maximum Service Temperature, Air 40.0 - 60.0 °C104 - 140 °FLong Term; ISO 2578
 100 °C212 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FISO 75-1/-2
Glass Transition Temp, Tg 125 °C257 °F10°C/min; ISO 11357-1/-2
Flammability, UL94 V-2V-2IEC 60695-11-10
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood contact
 
Descriptive Properties
AutomotiveInterior
Electricals & ElectronicsElectrical appliances
Food contactEU Requirements
FormGranules
Industry & Consumer goodsHousewares
MedicalUSP VI
PackagingCosmetics / Personal care
 Injection, stretch, blow molded containers
 Medical packaging
ProcessingInjection (stretch) blow molding
 Injection Molding
Product AttributesBarrier Properties
 Partially aromatic Polyamide
Special CharacteristicsTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 101 NC010 PA66
Envalior Durethan® T 40 ZS 000000 Partially aromatic polyamide
EMS-Grivory Grivory® G 21 PA6I/6T
Covestro Bayblend® FR 3030 Polycarbonate + ABS, Flame Retardant Grade
EMS-Grivory Grilamid® TR 90 NZ PAMACM12-I

PGRH319 / 157028

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.