MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 5052-H19 Foil
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: This alloy has good workability, very good corrosion resistance, high fatigue strength, weldability, and moderate strength. This leads to its use in aircraft fuel/oil lines, fuel tanks, other transportation areas, sheet metal work, appliances and lighting, wire, and rivets.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95052; ISO AlMg2.5; Aluminium 5052-H19 Foil; AA5052-H19 Foil; Al5052-H19
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.68 g/cc0.0968 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8888500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 111111
Hardness, Rockwell A 3737Converted from Brinell Hardness Value
Hardness, Rockwell B 5454Converted from Brinell Hardness Value
Hardness, Vickers 9999Converted from Brinell Hardness Value
Tensile Strength, Ultimate 330 MPa47900 psi
Tensile Strength, Yield 325 MPa47100 psi
Elongation at Break 4.0 %4.0 %Foil
Modulus of Elasticity 70.0 GPa10200 ksiAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus
Poissons Ratio 0.330.33
Shear Modulus 25.9 GPa3760 ksi
Shear Strength 200 MPa29000 psiCalculated value.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000499 ohm-cm
@Temperature 20.0 °C
0.00000499 ohm-cm
@Temperature 68.0 °F
AA; Typical
 
Thermal PropertiesMetricEnglishComments
CTE, linear  22.1 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.3 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.8 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 24.8 µm/m-°C
@Temperature 20.0 - 200 °C
13.8 µin/in-°F
@Temperature 68.0 - 392 °F
 25.7 µm/m-°C
@Temperature 20.0 - 300 °C
14.3 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.880 J/g-°C0.210 BTU/lb-°FEstimated from trends in similar Al alloys.
Thermal Conductivity 138 W/m-K960 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 607.2 - 649 °C1125 - 1200 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 607.2 °C1125 °FAA; Typical
Liquidus 649 °C1200 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 343 °C650 °Fholding at temperature not required
Hot-Working Temperature 260 - 510 °C500 - 950 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 95.7 - 97.7 %95.7 - 97.7 %As remainder
Chromium, Cr 0.15 - 0.35 %0.15 - 0.35 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 2.2 - 2.8 %2.2 - 2.8 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.25 %<= 0.25 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 5052-H32
Aluminum 5052-O
Aluminum 5052-H34
Aluminum 5052-H38
Aluminum 5052-H36

MA5052H19 / 9154

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.