MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Acetal Copolymer, Glass Bead Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Glass Bead Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.47 - 1.88 g/cc0.0531 - 0.0679 lb/in³Average value: 1.58 g/cc Grade Count:46
Filler Content 10.0 - 40.0 %10.0 - 40.0 %Average value: 20.0 % Grade Count:13
Water Absorption 0.100 - 0.500 %0.100 - 0.500 %Average value: 0.293 % Grade Count:19
Moisture Absorption at Equilibrium 0.160 - 0.200 %0.160 - 0.200 %Average value: 0.190 % Grade Count:5
Maximum Moisture Content  0.200 - 0.200
@Temperature 100 - 100 °C
0.200 - 0.200
@Temperature 212 - 212 °F
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.00300 - 0.0300 cm/cm0.00300 - 0.0300 in/inAverage value: 0.0156 cm/cm Grade Count:39
Linear Mold Shrinkage, Transverse 0.0150 - 0.0220 cm/cm0.0150 - 0.0220 in/inAverage value: 0.0184 cm/cm Grade Count:7
Melt Flow 4.00 - 23.0 g/10 min4.00 - 23.0 g/10 minAverage value: 15.0 g/10 min Grade Count:13
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 75.0 - 11475.0 - 114Average value: 106 Grade Count:14
Ball Indentation Hardness 182 - 202 MPa26400 - 29300 psiAverage value: 189 MPa Grade Count:3
Tensile Strength, Ultimate 31.0 - 103 MPa4500 - 15000 psiAverage value: 50.2 MPa Grade Count:37
 25.0 - 30.0 MPa
@Temperature 60.0 - 60.0 °C
3630 - 4350 psi
@Temperature 140 - 140 °F
Average value: 28.3 MPa Grade Count:3
Tensile Strength, Yield 35.0 - 55.0 MPa5080 - 7980 psiAverage value: 46.1 MPa Grade Count:10
Elongation at Break 1.20 - 40.0 %1.20 - 40.0 %Average value: 12.1 % Grade Count:43
 65.0 - 75.0 %
@Temperature 60.0 - 90.0 °C
65.0 - 75.0 %
@Temperature 140 - 194 °F
Average value: 85.0 % Grade Count:3
Elongation at Yield 5.00 - 8.50 %5.00 - 8.50 %Average value: 6.67 % Grade Count:6
 6.00 - 9.00 %
@Temperature 60.0 - 90.0 °C
6.00 - 9.00 %
@Temperature 140 - 194 °F
Average value: 7.58 % Grade Count:3
Modulus of Elasticity 2.00 - 8.96 GPa290 - 1300 ksiAverage value: 4.04 GPa Grade Count:31
 1.20 - 2.30 GPa
@Temperature 60.0 - 90.0 °C
174 - 334 ksi
@Temperature 140 - 194 °F
Average value: 1.67 GPa Grade Count:3
Flexural Yield Strength 55.2 - 152 MPa8000 - 22000 psiAverage value: 81.9 MPa Grade Count:37
Flexural Modulus 1.90 - 7.58 GPa276 - 1100 ksiAverage value: 3.66 GPa Grade Count:33
Izod Impact, Notched 0.267 - 3.50 J/cm0.500 - 6.56 ft-lb/inAverage value: 0.542 J/cm Grade Count:27
Izod Impact, Unnotched 1.07 - 6.94 J/cm2.00 - 13.0 ft-lb/inAverage value: 4.28 J/cm Grade Count:21
Izod Impact, Notched (ISO) 2.70 - 6.00 kJ/m²1.28 - 2.86 ft-lb/in²Average value: 4.55 kJ/m² Grade Count:6
 4.00 - 5.00 kJ/m²
@Temperature -30.0 - -30.0 °C
1.90 - 2.38 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.50 kJ/m² Grade Count:2
Charpy Impact Unnotched 2.00 - 6.00 J/cm²9.52 - 28.6 ft-lb/in²Average value: 3.92 J/cm² Grade Count:6
 3.80 - 3.80 J/cm²
@Temperature -20.0 - -20.0 °C
18.1 - 18.1 ft-lb/in²
@Temperature -4.00 - -4.00 °F
Average value: 3.80 J/cm² Grade Count:1
Charpy Impact, Notched 0.150 - 0.500 J/cm²0.714 - 2.38 ft-lb/in²Average value: 0.314 J/cm² Grade Count:16
 0.200 - 0.200 J/cm²
@Temperature -20.0 - -20.0 °C
0.952 - 0.952 ft-lb/in²
@Temperature -4.00 - -4.00 °F
Average value: 0.200 J/cm² Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 - 1.00e+16 ohm-cm1.00e+14 - 1.00e+16 ohm-cmAverage value: 1.64e+15 ohm-cm Grade Count:23
Surface Resistance 1.00e+14 - 1.00e+16 ohm1.00e+14 - 1.00e+16 ohmAverage value: 4.75e+15 ohm Grade Count:11
Dielectric Constant 3.80 - 4.903.80 - 4.90Average value: 4.34 Grade Count:5
Dielectric Strength 17.7 - 30.0 kV/mm450 - 762 kV/inAverage value: 22.5 kV/mm Grade Count:9
Dissipation Factor 0.00600 - 0.01150.00600 - 0.0115Average value: 0.00980 Grade Count:5
Comparative Tracking Index 500 - 600 V500 - 600 VAverage value: 578 V Grade Count:9
 
Thermal PropertiesMetricEnglishComments
CTE, linear 45.0 - 90.0 µm/m-°C25.0 - 50.0 µin/in-°FAverage value: 65.3 µm/m-°C Grade Count:4
Melting Point 162 - 178 °C324 - 352 °FAverage value: 167 °C Grade Count:15
Maximum Service Temperature, Air 80.0 °C176 °FAverage value: 80.0 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 141 - 177 °C285 - 350 °FAverage value: 161 °C Grade Count:22
Deflection Temperature at 1.8 MPa (264 psi) 100 - 163 °C212 - 325 °FAverage value: 126 °C Grade Count:35
Vicat Softening Point 150 - 165 °C302 - 329 °FAverage value: 154 °C Grade Count:8
Flammability, UL94 HBHBGrade Count:36
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 230 °C350 - 446 °FAverage value: 199 °C Grade Count:17
Nozzle Temperature 190 - 220 °C374 - 428 °FAverage value: 205 °C Grade Count:3
Melt Temperature 165 - 220 °C329 - 428 °FAverage value: 195 °C Grade Count:21
Mold Temperature 50.0 - 120 °C122 - 248 °FAverage value: 90.4 °C Grade Count:38
Injection Velocity 20.0 - 50.0 mm/sec0.787 - 1.97 in/secAverage value: 35.0 mm/sec Grade Count:4
Drying Temperature 80.0 - 121 °C176 - 250 °FAverage value: 101 °C Grade Count:24
Moisture Content 0.100 - 0.150 %0.100 - 0.150 %Average value: 0.144 % Grade Count:9
Dew Point -31.7 °C-25.0 °FAverage value: -31.7 °C Grade Count:8
Injection Pressure 30.0 - 118 MPa4350 - 17100 psiAverage value: 79.4 MPa Grade Count:23

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, PTFE Filled

O1255 / 77844

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.