MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Goodfellow TPX® MX002O Polymethylpentene
Categories: Polymer; Thermoplastic; Polymethylpentene (PMP); Polymethylpentene, Molded

Material Notes: This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.

TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics and good high frequency electrical and valuable acoustic/ultrasonic properties. Applications include medical and laboratory apparatus, microwave components and cookware and electronic components.

Information provided by Goodfellow. TPX® is a trademark of Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.833 g/cc0.0301 lb/in³ASTM D1505
Water Absorption <= 0.010 %<= 0.010 %ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inMCI Method 2
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inMCI Method 2
Melt Flow 21 g/10 min
@Load 5.00 kg,
Temperature 260 °C
21 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Spiral Flow 56.0 cm22.0 inMCI Method 1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 4242ASTM D785
Tensile Strength 10.0 MPa1450 psiASTM D638
Tensile Strength, Yield 21.0 MPa3050 psiASTM D638
Elongation at Break 60 %60 %ASTM D638
Tensile Modulus 0.880 GPa128 ksiASTM D638
Flexural Strength 27.0 MPa3920 psiASTM D790
Flexural Modulus 0.660 GPa95.7 ksiASTM D790
Izod Impact, Notched 0.280 J/cm0.525 ft-lb/inASTM D256
Izod Impact, Unnotched (ISO) 129 kJ/m²61.4 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.12.1ASTM D150
Dielectric Strength 65.0 kV/mm1650 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 117 µm/m-°C65.0 µin/in-°FASTM E831
Melting Point 224 °C435 °FDSC Peak; JIS K7121
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FASTM D648
Vicat Softening Point 165 °C329 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.461.46ASTM D542
Haze 1.2 %1.2 %ASTM D1003
Transmission, Visible 93 %93 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene
Akro-Plastic Akrotek® PEEK natural (5184) PEEK, Dry
Mitsui TPX® RT18 XB Methylpentene Copolymer

PGOODF226 / 135578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.