MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Tecoflex® EG-100A TPU - Clear
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Medical Grade Aliphatic Polyether-based Thermoplastic Polyurethane (TPU)

Features: offers an inherent ultraviolet (UV) stability that resists yellowing by aging and sterilization, good mechanical properties and can be color-matched

Process: Extrusion and Injection Molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm0.0060 - 0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494ASTM D2240
Tensile Strength, Ultimate 56.5 MPa8200 psiASTM D412
Elongation at Break 370 %370 %ASTM D412
100% Modulus 11.0 MPa
@Strain 100 %
1600 psi
@Strain 100 %
ASTM D412
200% Modulus 20.7 MPa
@Strain 200 %
3000 psi
@Strain 200 %
ASTM D412
300% Modulus 38.6 MPa
@Strain 300 %
5600 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.0689 GPa10.0 ksiASTM D790
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 162.7 °C324.9 °FInjection
Front Barrel Temperature 176.6 °C349.9 °FInjection
Nozzle Temperature 182.2 °C360.0 °FInjection
Zone 1 176.6 °C349.9 °FExtrusion
Zone 2 182.8 °C361.0 °FExtrusion
Zone 3 187.7 °C369.9 °FExtrusion
Zone 4 187.7 °C369.9 °FExtrusion
Adapter Temperature 187.7 °C369.9 °FExtrusion
Die Temperature 193.3 °C379.9 °FExtrusion
Melt Temperature <= 210 °C<= 410 °FInjection
Mold Temperature 10.0 - 43.3 °C50.0 - 110 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Tecoflex® EG-80A TPU - Clear
Arkema Pebax® Rnew® 80R53 SP 02 TPA
Arkema Pebax® Rnew® 30R51 SA 01 TPA
Arkema Pebax® MF 5080 TPA
Lubrizol LifeSciences Carbothane® PC-3575A TPU – Clear Aliphatic

PLUBR9048 / 203615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.