MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Orion Engineered Carbons PRINTEX® XE 2B Conductive Carbon Black
Categories: Carbon; Carbon Black

Material Notes: Specialty conductive carbon black

Information provided by Orion Engineered Carbons.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Oil Absorption 420 %420 %(ml/100 g); ASTM D 2414
Loss On Ignition <= 2.0 %<= 2.0 %Heating Loss; ASTM D 1509
Specific Surface Area 1000 m²/g1000 m²/gStatistical thickness surface area; ASTM D 6556
Iodine Absorption Number 11251125mg/g; ASTM D 1510
 
Descriptive Properties
Fines< 12.0 %ASTM D 1508
Individual Pellet Hardness< 20 gASTM D 5230, average 1.4 - 1.7 mm
Sieve Residue< 500 ppmASTM D 1514

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Orion Engineered Carbons PRINTEX® L6 Beads Conductive Carbon Black
Kraton® D1184 (SB)n Branched Copolymer
A. Schulman ComAlloy Comshield® 104 Homopolymer Polypropylene, Electrically Conductive - Carbon Black Filled
Graphite, Carbon, C
TIMCAL ENSACO™ 350G Conductive Carbon Black

EORION939 / 159763

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.