MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexWeb® HDC-660 - 3/16 - 17.5 (R2) Heavy Density Core
Categories: Other Engineering Material; Composite Core Material; Composite Fibers; Polymer; Thermoset; Carbon Fiber/Thermoset Composite

Material Notes: Designation: Material-Cell Size (inches)-Density
HexWeb® HDC is a fabric reinforced honeycomb, typically made from either fiberglass or carbon prepreg. A thermosetting node adhesive is used with either a thermoplastic or thermoset resin for the web impregnations. The product was developed for use in temperatures up to 500°F. Depending on the constituent resin system, the product may be suitable for short exposures at higher temperatures.

Features: High compression strength non-metallic honeycomb available; Formability tailored to customer's needs; Low-moisture pickup; High thermal stability, very low coefficient of thermal expansion; Proven history in service; High corrosion resistance.
Applications: HexWeb® HDC is used in sandwich structure as a replacement for potting compound in hard points or where extremely high compressive or shear strength is required. Using HexWeb® HDC in lieu of potting compound reduces process steps, improves part quality and reduces weight in the overall structure.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.280 g/cc0.0101 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength 26.9 MPa3900 psiStabilized
Shear Strength 7.58 MPa1100 psiLong Beam Shear, W Direction
 13.4 MPa1950 psiLong Beam Shear, L Direction

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 5250-4 BMI Prepreg System with IM7-6K-5HS Woven Carbon Fiber
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg
Hexcel® HexWeb® HDC - 3/16 - 16.0 (R2) Heavy Density Core
Hexcel® Fibrelam® 2000 Grade 1 Panels for Aircraft Flooring
Solvay CYCOM® 381 Epoxy Prepreg with IM7 Uni-graphite and 148FAW Epoxy

PHEXC388 / 98859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.