MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil TPE U75 Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: A completely recyclable, polypropylene-based, soft, rubber-like black material that can be processed on conventional thermoplastics equipment for injection molding, extrusion, thermoforming or blow molding. This material can be used in a wide range of applications, with use temperatures up to 90°C (195°F).

Features: Recyclable Material

Agency Ratings: EU 2003/11/EC

RoHS Compliant

Appearance: Black

    Processing Method:
  • Blow Molding
  • Coextrusion
  • Extrusion
  • Extrusion Blow Molding
  • Injection Blow Molding
  • Injection Molding
  • Multi Injection Molding
  • Profile Extrusion
  • Sheet Extrusion
  • Thermoforming

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Melt Flow  21 g/10 min
@Load 10.0 kg,
Temperature 230 °C
21 g/10 min
@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
 21 g/10 min
@Load 10.0 kg,
Temperature 230 °C
21 g/10 min
@Load 22.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75
@Thickness 2.00 mm,
Temperature 23.0 °C
75
@Thickness 0.0787 in,
Temperature 73.4 °F
ISO 868
Tensile Stress at Strain  2.90 MPa
@Strain 100 %,
Temperature 2.00 °C
421 psi
@Strain 100 %,
Temperature 35.6 °F
ASTM D412
 2.90 MPa
@Strain 100 %,
Temperature 2.00 °C
421 psi
@Strain 100 %,
Temperature 35.6 °F
ISO 37

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
IBC Advanced Alloys 2.6% BeAl Beryllium Aluminum Master Alloy
Supreme Petrochem SPEXP 44 Antistatic Polystyrene
Beryllium Aluminate, BeAl2O4
Materion AlBeMet® AM 162 HIP'd Billet, Annealed
Iron (II) Chromite, FeCr2O4

PZZEXX990 / 209778

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.