MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³
Linear Mold Shrinkage, Flow 0.011 - 0.014 cm/cm0.011 - 0.014 in/in
Linear Mold Shrinkage, Transverse 0.0115 - 0.0145 cm/cm0.0115 - 0.0145 in/in
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break  >= 100 %
@Temperature 23.0 °C
>= 100 %
@Temperature 73.4 °F
 >= 100 %
@Temperature 60.0 °C
>= 100 %
@Temperature 140 °F
 >= 100 %
@Temperature 90.0 °C
>= 100 %
@Temperature 194 °F
Elongation at Yield  8.0 %
@Temperature 23.0 °C
8.0 %
@Temperature 73.4 °F
 10 %
@Temperature 60.0 °C
10 %
@Temperature 140 °F
Tensile Modulus  0.500 GPa
@Temperature 90.0 °C
72.5 ksi
@Temperature 194 °F
 1.00 GPa
@Temperature 60.0 °C
145 ksi
@Temperature 140 °F
 2.50 GPa
@Temperature 23.0 °C
363 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 400 V400 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 110 °C230 °F
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °F
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °F
Vicat Softening Point 80.0 °C
@Load 5.00 kg
176 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 240 °C392 - 464 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 80.0 - 90.0 °C
@Time 10800 sec
176 - 194 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
LATI Latamid 66 PA 66
Versalis Riblene® MP 30 Low Density Polyethylene - Injection Molding
Celanese Celcon® GB25 POM, 25% Glass Reinforced
Celanese Celcon® GB10 POM, 10% Glass Reinforced

PLATH9772 / 177468

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.