Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike applications. It is available with knitted nylon, matt nylon and metal foils, in a choice of weights to suit the wide range of applications. Redux 330 has excellent structural bonding performance and exceeds the requirements of BMS-8-245.Areal Weights: 0.35, 0.05, 0.08 psf. Features: Ideal for composite to composite bonding (no metallic fiber); Suitable for co-cure with 350°F prepreg systems; Good structural performance and service temperature to 270°F; Low volatile content (solventless production process); Excellent environmental resistance; High toughness; Light tack and good drapability; Contains carrier for glueline thickness control and for improved adhesive handling. Applications: Structural Composite Bonding |