MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sharadaa Ceramics REFINSUL 4 Insulating Castables Medium/High Purity
Categories: Ceramic

Material Notes: Manufacturer produces Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistance property.

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 g/cc0.0181 lb/in³Dried at 110°C
Grain Size <= 6000 µm<= 6000 µm
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.00441 GPa
@Temperature 1100 °C
0.640 ksi
@Temperature 2010 °F
 0.00931 GPa
@Temperature 110 °C
1.35 ksi
@Temperature 230 °F
 0.0108 GPa
@Temperature 1500 °C
1.57 ksi
@Temperature 2730 °F
Compressive Strength  0.0981 MPa
@Temperature 1000 °C
14.2 psi
@Temperature 1830 °F
Cold Crushing
 0.196 MPa
@Temperature 110 °C
28.4 psi
@Temperature 230 °F
Cold Crushing
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.105 W/m-K0.729 BTU-in/hr-ft²-°F
 1.28 W/m-K8.88 BTU-in/hr-ft²-°F
 1.37 W/m-K9.51 BTU-in/hr-ft²-°F
 1.45 W/m-K10.1 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 11 %11 %
 
Descriptive Properties
Permanent Linear Change<-0.06%800°C
 <-0.08%1500°C
 <-0.12%1100°C
 -0.8 - 0.8%1000°C
Refractoriness<1800°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Firelite 1230 Thermal Ceramic
Thermal Ceramics BTU-GUE
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity
Mid-Mountain Materials CERMEX® PR1000-M Premium Grade Thermal Insulation Paper
Anderman Ceramics EREY99 Yttrium Oxide

CSHARA033 / 130196

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.