(PC+ABS)-Blend; flame retardant; Vicat/B 120 temperature = 103 °C; improved chemical and very good hydrolysis resistance; HDT/A >= 85 °C; UL recognition 94 V-0 at 1.5 mm; Glow wire test: 960 °C at 2.0 mm; good light stabilityAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |