MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zytel® 73G45 BK263 PA6-GF45
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: 45% Glass Reinforced Polyamide 6

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³DAM; ISO 1183
Melt Density 1.33 g/cc
@Temperature 270 °C
0.0480 lb/in³
@Temperature 518 °F
Water Absorption 4.9 %
@Thickness 2.00 mm
4.9 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.70 %
@Thickness 2.00 mm
1.70 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Number 150 cm³/g1.50 dl/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 145 MPa21000 psi50% RH; ISO 527-1/-2
 215 MPa31200 psiDAM; ISO 527-1/-2
Elongation at Break 3.0 %3.0 %DAM; ISO 527-1/-2
 5.0 %5.0 %50% RH; ISO 527-1/-2
Tensile Modulus 9.00 GPa1310 ksi50% RH; ISO 527-1/-2
 14.2 GPa2060 ksiDAM; ISO 527-1/-2
Poissons Ratio 0.330.33DAM
 0.340.3450% RH
Izod Impact, Notched (ISO)  17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 22.0 kJ/m²
@Temperature 23.0 °C
10.5 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  1.90 J/cm²
@Temperature 23.0 °C
9.04 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 2.40 J/cm²
@Temperature 23.0 °C
11.4 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 9400 MPa1.36e+6 psi1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 7300 MPa1.06e+6 psi1000h; 50% RH; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 500 V500 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 2.10 J/g-°C
@Temperature 270 °C
0.502 BTU/lb-°F
@Temperature 518 °F
Melt
Thermal Conductivity 0.260 W/m-K
@Temperature 270 °C
1.80 BTU-in/hr-ft²-°F
@Temperature 518 °F
Melt
Melting Point 221 °C430 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 218 °C424 °FDAM; ISO 75-1/-2
Glass Transition Temp, Tg 15.0 °C59.0 °F10°C/min; 50% RH; ISO 11357-1/-2
 55.0 °C131 °F10°C/min; DAM; ISO 11357-1/-2
Flame Spread 44.0 mm/min
@Thickness 1.00 mm
1.73 in/min
@Thickness 0.0394 in
DS; ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °FOptimum, Injection
 260 - 280 °C500 - 536 °FRange, Injection
Mold Temperature 70.0 - 120 °C158 - 248 °FInjection
 100 °C212 °FOptimum, Injection
Ejection Temperature 210 °C410 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6,GF45,M1CGR,S14-140
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA6-GF45<ISO 11469
PolymerPA6-GF45
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA6-GF45ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 73G45L NC010 PA6-GF45
Envalior Novamid® 1013G45 1 NA PA6-GF45
Envalior Novamid® 1013GH45 1 NA/BK701 PA6-GF45
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
BASF Ultramid® 8351 HS BK 106 PA6 (Dry)

PDSX5361 / 198001

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.