MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nanocyl NANOCYL™ NC1000 Single-Wall Isolated and Bundled Carbon Nanotubes - Research grade
Categories: Carbon

Material Notes: NANOCYL™ NC1000 series single-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 70% carbon to produce the 1100 grade. This grade is then functionalized with COOH to produce the 1101 grade. These products are available in 1 to 10 gram order quantities.

A primary interest is in applications requiring high specific surface area (BET >1000 m²/g).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 - 2.00 g/cc1.30 - 2.00 g/cc
Specific Surface Area >= 1000 m²/g>= 1000 m²/gBET
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 10 %10 %
Tensile Modulus 1000 GPa145000 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.00001 - 0.0001 ohm-cm0.00001 - 0.0001 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity >= 3000 W/m-K>= 20800 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C >= 70 %>= 70 %TGA
 
Descriptive Properties
Average Diameter2 nanometersHRTEM, Raman
Average Lengthseveral micronsTEM
-COOH Functionalization<5%XPS
Metal Oxide<30%TGA (includes carbon shells)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Copper, Cu; Cold-Worked
Graphite, Carbon, C
Copper, Cu; Cold Drawn
Diamond, Natural

ENANOC951 / 108918

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.