MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Data provided by Carpenter Technology Corporation.

Annealing followed by water quench and low stress grinding prior to tensile testing.

Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur CCM Plus alloy is a wrought powder metallurgy product produced by vacuum induction melting (VIM) followed by inert gas atomization and hot isostatic pressing to produce 100% dense billets. These billets are then processed by conventional steel-making practices to make finished products.

BioDur™ and CCM Plus™ are trademarks of Carpenter Technology Corporation.

Key Words: ASTM F799; ASTM F1537; ISO 5832-4; ISO 5832-12
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.28 g/cc0.299 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 369369Estimated from Rockwell C for Brinell test with 3000 kg load, 10 mm ball.
Hardness, Knoop 403403Estimated from Rockwell C
Hardness, Rockwell C 4040
Hardness, Vickers 386386Estimated from Rockwell C
Tensile Strength, Ultimate 1392 MPa201900 psi
Tensile Strength, Yield 806 MPa
@Strain 0.2 %
117000 psi
@Strain 0.2 %
Elongation at Break 29 %29 %in 4D
Reduction of Area 25 %25 %
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.8 µm/m-°C
@Temperature 0.000 - 100 °C
7.11 µin/in-°F
@Temperature 32.0 - 212 °F
 13.1 µm/m-°C
@Temperature 25.0 - 300 °C
7.30 µin/in-°F
@Temperature 77.0 - 572 °F
 14.7 µm/m-°C
@Temperature 25.0 - 700 °C
8.18 µin/in-°F
@Temperature 77.0 - 1290 °F
 16.92 µm/m-°C
@Temperature 25.0 - 1000 °C
9.400 µin/in-°F
@Temperature 77.0 - 1830 °F
Specific Heat Capacity  0.452 J/g-°C
@Temperature 23.0 °C
0.108 BTU/lb-°F
@Temperature 73.4 °F
 0.590 J/g-°C
@Temperature 600 °C
0.141 BTU/lb-°F
@Temperature 1110 °F
 0.673 J/g-°C
@Temperature 1100 °C
0.161 BTU/lb-°F
@Temperature 2010 °F
Thermal Conductivity  12.766 W/m-K
@Temperature 23.0 °C
88.596 BTU-in/hr-ft²-°F
@Temperature 73.4 °F
 25.264 W/m-K
@Temperature 600 °C
175.33 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 35.022 W/m-K
@Temperature 1177 °C
243.05 BTU-in/hr-ft²-°F
@Temperature 2151 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.20 - 0.30 %0.20 - 0.30 %
Chromium, Cr 26 - 30 %26 - 30 %
Cobalt, Co 66 %66 %as remainder
Molybdenum, Mo 5.0 - 7.0 %5.0 - 7.0 %
Nitrogen, N 0.15 - 0.20 %0.15 - 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr
ATI Allvac® Nickelvac® TJA-1537™ UNS R31537 & UNS R31538 Nickel Superalloy, Warm Worked
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 2 hr

NCAR33 / 15623

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.