MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total 7620Z Polypropylene, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Random copolymer for injection molding

Clarity - FINA 7620Z exhibits high clarity in molded parts.

Impact - FINA 7620Z produces molded parts with improved impact compared with parts molded from polypropylene homopolymers.

Antistat - FINA 7620Z contains an antistat to help protect molded parts from dust accumulation.

FDA - FINA 7620Z complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 7620Z is recommended for injection molding housewares, hinged closures and other items calling for good impact, flexibility, and clarity.

Processing - FINA 7620Z resin processes on conventional injection molding equipment with typical melt temperatures of 390-450°F (200- 232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 11 g/10 min11 g/10 minASTM D1238L
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D288A
Tensile Strength, Ultimate 22.1 MPa3210 psiASTM D638
Elongation at Break 11 %11 %ASTM D638
Modulus of Elasticity 0.760 GPa110 ksiASTM D638
Flexural Modulus 0.620 GPa89.9 ksiASTM D790
Izod Impact, Notched 0.694 J/cm1.30 ft-lb/inASTM D256A
Izod Impact, Unnotched NBNBASTM D256A
Impact Test 23.7 J
@Thickness 3.17 mm
17.5 ft-lb
@Thickness 0.125 in
Drop Impact, plaques. Fina API test
 
Thermal PropertiesMetricEnglishComments
Melting Point 145 °C293 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 232 °C392 - 450 °FInjection

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® NA206000 Low Density Polyethylene
LyondellBasell Alathon® L5885 High Density Polyethylene
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene
LyondellBasell Pro-fax SA861 Polypropylene Random Copolymer, Cast Film Extrusion
LyondellBasell Pro-fax 6523 Polypropylene Homopolymer, General Purpose

PFIN97 / 38427

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.