System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose
Categories:
Polymer
;
Thermoplastic
;
Polystyrene (PS)
;
Syndiotactic Polystyrene (SPS)
;
Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
Material Notes:
Feature: Injection Molding, sPS+GF30%, General Purpose
Application: Pump Units, Pick-up Lends Holder, etc.
CAS No. 9003-53-6 and 65997-17-3
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.25
g/cc
1.25
g/cc
ASTM D792
Maximum Moisture Content
0.020
0.020
Injection Molding
Linear Mold Shrinkage, Flow
0.0030
-
0.0090
cm/cm
@Thickness 3.20 mm
0.0030
-
0.0090
in/in
@Thickness 0.126 in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
118
MPa
@Thickness 3.20 mm
17100
psi
@Thickness 0.126 in
5mm/min; ASTM D638
Elongation at Break
2.0 %
@Thickness 3.20 mm
2.0 %
@Thickness 0.126 in
5mm/min; ASTM D638
Flexural Yield Strength
177
MPa
@Thickness 3.20 mm
25600
psi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Flexural Modulus
8.83
GPa
@Thickness 3.20 mm
1280
ksi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Izod Impact, Notched
0.883
J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.65
ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Dielectric Strength
35.0
kV/mm
@Thickness 1.00 mm
889
kV/in
@Thickness 0.0394 in
ASTM D149
Arc Resistance
120
-
180
sec
120
-
180
sec
ASTM D495
Comparative Tracking Index
500
-
600
V
500
-
600
V
Solution A; IEC 60112
Hot Wire Ignition, HWI
15
-
30
sec
@Thickness >=3.00 mm
15
-
30
sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI
30
-
60
arcs
@Thickness 3.00 mm
30
-
60
arcs
@Thickness 0.118 in
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
260
°C
@Thickness 6.40 mm
500
°F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
>=
220
°C
@Thickness 6.40 mm
>=
428
°F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical
50.0
°C
@Thickness >=1.50 mm
122
°F
@Thickness >=0.0591 in
50.0
°C
@Thickness >=3.00 mm
122
°F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact
50.0
°C
@Thickness >=1.50 mm
122
°F
@Thickness >=0.0591 in
50.0
°C
@Thickness >=3.00 mm
122
°F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact
50.0
°C
@Thickness >=1.50 mm
122
°F
@Thickness >=0.0591 in
50.0
°C
@Thickness >=3.00 mm
122
°F
@Thickness >=0.118 in
Flammability, UL94
HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
HB
@Thickness >=3.00 mm
HB
@Thickness >=0.118 in
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
270
-
290
°C
518
-
554
°F
Injection Molding
Middle Barrel Temperature
280
-
310
°C
536
-
590
°F
Injection Molding
Front Barrel Temperature
290
-
310
°C
554
-
590
°F
Injection Molding
Nozzle Temperature
280
-
310
°C
536
-
590
°F
Injection Molding
Melt Temperature
280
-
310
°C
536
-
590
°F
Injection Molding
Mold Temperature
80.0
-
150
°C
176
-
302
°F
Injection Molding
Drying Temperature
80.0
-
100
°C
176
-
212
°F
Injection Molding
Dry Time
3.00
-
5.00
hour
3.00
-
5.00
hour
Injection Molding
Screw Speed
40
-
80
rpm
40
-
80
rpm
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Entec Hyrene® PSCRY 14 General Purpose Polystyrene
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled
LG Chemical LUSEP SP2306F SPS+GF30%, Flame Retardant
PLAY186 / 148196
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.