MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Medalist® MD-84368 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-84300 series are high performance thermoplastic elastomer designed specifically for extrusion and injection molded electrical applications in the medical and healthcare industry. The Medalist MD-84300 series are a better alternative to traditional TPVs used in such applications. Medalist MD-84368 is a medium hardness, low density grade with good electrical properties and can be sterilized by autoclave, ETO, or gamma radiation.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Electrically Insulating; Ethylene Oxide Sterilizable; Good Color Stability; Good Colorability; Good Sterilizability; Halogen Free; High Tensile Strength; Low Flow; Low Specific Gravity; Medium Hardness; Radiation Sterilizable; Slip

Uses: Flexible Jacketing; Medical/Healthcare Applications; Pharmaceuticals; Rubber Replacement; Wire & Cable Applications

Agency Ratings: ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  68
@Time 5.00 sec
68
@Time 0.00139 hour
ASTM D2240
 70
@Time 1.00 sec
70
@Time 0.000278 hour
ASTM D2240
Tensile Strength at Break 18.3 MPa2650 psiASTM D412
 12.6 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
1830 psi
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D412
 23.0 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
3340 psi
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D412
Tensile Stress at Strain  2.62 MPa
@Strain 100 %
380 psi
@Strain 100 %
ASTM D412
 4.55 MPa
@Strain 300 %
660 psi
@Strain 300 %
ASTM D412
Elongation at Break 700 %700 %ASTM D412
 651 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
651 %
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D412
 696 %
@Treatment Temp. 136 °C,
Time 605000 sec
696 %
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D412
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  3.90e+15 ohm-cm
@Temperature 50.0 °C
3.90e+15 ohm-cm
@Temperature 122 °F
ASTM D257
 4.30e+16 ohm-cm
@Temperature 22.8 °C
4.30e+16 ohm-cm
@Temperature 73.0 °F
ASTM D257
Dielectric Constant 2.29
@Frequency 1000 Hz
2.29
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 47.2 kV/mm1200 kV/inASTM D149
Dissipation Factor 0.00086
@Frequency 1000 Hz
0.00086
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
NT
Oxygen Index 19 %19 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 221 - 229 °C430 - 445 °FMelt, Injection
Rear Barrel Temperature 199 - 216 °C390 - 420 °FInjection
Middle Barrel Temperature 213 - 221 °C415 - 430 °FInjection
Front Barrel Temperature 221 - 227 °C430 - 440 °FInjection
Nozzle Temperature 221 - 229 °C430 - 445 °FInjection
Zone 1 193 - 210 °C380 - 410 °FExtrusion
Zone 2 199 - 216 °C390 - 420 °FExtrusion
Zone 3 213 - 221 °C415 - 430 °FExtrusion
Zone 4 213 - 221 °C415 - 430 °FExtrusion
Zone 5 221 - 229 °C430 - 445 °FExtrusion
Die Temperature 221 - 229 °C430 - 445 °FExtrusion
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical KEYFLEX BT 1028D Ester Type TPE
Teknor Apex Medalist® MD-8431 Thermoplastic Elastomer
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer
Overview of materials for Polypropylene, Flame Retardant

PTEKNQ0752 / 237243

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.