MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBAFLEX S 70 A.01 TPE-S, Shore A70, translucent
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: TPE-S

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.017 cm/cm0.017 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070
Tensile Strength at Break 10.6 MPa1540 psiISO 527-1
Elongation at Break 710 %710 %ISO 527-1
 
Descriptive Properties
Resin TypeTPE-S

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Denka REOMER G G8250 Thermoplastic Elastomer, For Injection Molding
Multibase TPSiV® 4100-70A Thermoplastic Silicone Vulcanizate
Buckeye Polymers BP FLEX A 7010 UR Injection Grade TPE
BASF Elastollan® C 70 A HPM TPUR
Barlog Plastics KEBAFLEX SG 50 A.1 black TPE-S, Shore A50, black

PBARLO882 / 149900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.