MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shin-Etsu Silicones LIMS™ KEG2002-60A/B Elastomer
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes:

Information Provided by Shin-Etsu Silicones of America, Inc.

Key Words: LSR, Liquid Silicone Rubber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/cc
Viscosity 700000 cP700000 cPA
 700000 cP700000 cPB
Linear Mold Shrinkage 0.026 cm/cm0.026 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060
Tensile Strength 10.0 MPa1450 psi
Elongation at Yield 410 %410 %
100% Modulus 2.67 MPa
@Strain 100 %
387 psi
@Strain 100 %
Tear Strength 42.0 kN/m240 pli
Compression Set  8.0 %
@Temperature 200 °C,
Time 14400 sec
8.0 %
@Temperature 392 °F,
Time 4.00 hour
 34 %
@Temperature 150 °C,
Time 3600 sec
34 %
@Temperature 302 °F,
Time 1.00 hour
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 min
@Temperature 150 °C
0.0833 hour
@Temperature 302 °F
Press Cure
 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
Post Cure
 
Descriptive Properties
AppearanceTranslucent
Cure Rate28T10 (302°F, ODR)
 40T90 (302°F, ODR)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QM 258 60 Shore A, Addition Cure Moldmaking Material
Garlock 502 Silicone Sheet Rubber
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III
CHT Group QSil 960 55 Shore A, Condensation Cure for Potting Applications
Shin-Etsu Silicones LIMS™ KEG2000-60A/B Elastomer

PSHIN019 / 103846

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.