MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

GEHR Plastics PVC-ELS Polyvinylchloride, Electrically Conductive Grade
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuous operating temperature is from -15°C to 60°C. It can also be easily solvent, cemented and welded.

Properties include:

  • High mechanical strength, tensile strength and hardness
  • Good insulation properties for electronics
  • High chemical resistance
  • Self-extinguishing
  • Low water absorption
  • Easy to varnish and glue
  • Low impact strength
  • Limited weather resistance
Applications include:
  • Pumps and valve body
  • Gaskets
  • Bearing cages
  • Pipe lines
  • Hand pump pipes
  • Brush basic body
  • Parts in the dental medicine
  • Seat strips
  • Pipes for the mounting of kerfs
  • Lamp box
PVC-ELS has improved electronical conductivity.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 34.99 MPa5075 psiASTM D638
Elongation at Break 35 %35 %ASTM D638
Modulus of Elasticity 2.16 GPa313 ksiASTM D790
Izod Impact, Notched 1.01 J/cm1.90 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+6 ohm-cm<= 1.00e+6 ohm-cmASTM D257
Surface Resistance <= 1000 ohm<= 1000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.186 W/m-K
@Temperature 20.0 °C
1.29 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
ASTM C177
Maximum Service Temperature, Air 50.0 °C122 °FUL 746B
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C130 °FASTM D648
Vicat Softening Point 65.0 °C149 °FVST/B/50; ASTM D1525
Minimum Service Temperature, Air -10.0 °C14.0 °FUL 746B
Flammability, UL94 V-0V-0self assessment without test reports; UL 94
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistancelimited
Bondabilityyes
CKW Resistanceno
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistanceno
Resistance Against Hot Waterno

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
440C Martensitic Stainless Steel (UNS S44004)
AISI 1095 Steel, normalized at 900°C (1650°F)
Overview of materials for PVC, Rigid Grade
Overview of materials for PVC, Molded
Suqian Unitechem Light Stabilizer 944

PGEHR003 / 79840

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.