MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta NP502 Glass Fabric  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Low cost woven glass fabric epoxy laminate. Provides NEMA grade FR-4 properties at lower cost than NP130.MIL-I-24768/27, type GEE-F and the obsolete MIL-P-18177D, type GEE. Material is available in green color only.

Thickness Tested: 0.0620”, 0.125" and 0.500”.

Key Words: Micarta
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.85 g/cc
@Thickness 1.57 mm
1.85 g/cc
@Thickness 0.0620 in
ASTM D792
Moisture Absorption at Equilibrium 0.20 %
@Thickness 1.57 mm
0.20 %
@Thickness 0.0620 in
ASTM D229
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 105 - 125
@Thickness 1.57 mm
105 - 125
@Thickness 0.0620 in
ASTM D785
Tensile Strength, Yield  221 MPa
@Thickness 1.57 mm
32000 psi
@Thickness 0.0620 in
CW; ASTM D638
 276 MPa
@Thickness 1.57 mm
40000 psi
@Thickness 0.0620 in
LW; ASTM D638
Modulus of Elasticity  19.3 GPa
@Thickness 1.57 mm
2800 ksi
@Thickness 0.0620 in
CW; ASTM D229
 22.1 GPa
@Thickness 1.57 mm
3200 ksi
@Thickness 0.0620 in
LW; ASTM D229
Flexural Strength  359 MPa
@Thickness 1.57 mm
52000 psi
@Thickness 0.0620 in
CW; ASTM D790
 448 MPa
@Thickness 1.57 mm
65000 psi
@Thickness 0.0620 in
LW; ASTM D790
Compressive Strength 455 MPa
@Thickness 12.7 mm
66000 psi
@Thickness 0.500 in
ASTM D695
Shear Strength 148 MPa
@Thickness 15.7 mm
21500 psi
@Thickness 0.620 in
ASTM D732
Izod Impact, Unnotched  3.90 J/cm
@Thickness 12.7 mm
7.30 ft-lb/in
@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
 4.22 J/cm
@Thickness 12.7 mm
7.90 ft-lb/in
@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.5
@Thickness 1.57 mm
4.5
@Thickness 0.0620 in
Cond D-24/23; ASTM D150
Dielectric Breakdown  65000 V
@Thickness 1.57 mm
65000 V
@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S/S
 66000 V
@Thickness 1.57 mm
66000 V
@Thickness 0.0620 in
Cond A; ASTM D229 S/S
Dissipation Factor 0.020
@Thickness 1.57 mm
0.020
@Thickness 0.0620 in
Cond D-24/23; ASTM D150
Arc Resistance 120 sec
@Thickness 3.17 mm
120 sec
@Thickness 0.125 in
ASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C
@Thickness 1.57 mm,
Temperature 20.0 °C
5.56 µin/in-°F
@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 13.0 µm/m-°C
@Thickness 1.57 mm,
Temperature 20.0 °C
7.22 µin/in-°F
@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Maximum Service Temperature, Air 140 °C284 °F
Glass Transition Temp, Tg 140 °C284 °FTg
Flammability, UL94 V-0
@Thickness 1.57 mm
V-0
@Thickness 0.0620 in
 
Descriptive Properties
Bond Strength2100 lb0.5", ASTM D229
ColorGreen

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elmet-Starck Pure Molybdenum GME Glass Melting Electrodes
Norplex-Micarta RT509 Melamine Fiber Glass Laminate Tube, NEMA G-9
AISI 1018 Steel, cold drawn
H.C. Starck Amperit® 551.059 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni)
H.C. Starck Amperit® 518.002 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)

PNORPN546 / 48131

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.