MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Accella Bayseal® OCX Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Characterization: Bayseal open-cell X (OCX) is a spray-applied polyurethane foam (SPF) insulation.

Properties / Applications: Bayseal open-cell X (OCX) spray-applied polyurethane foam insulation is produced with a two component, low density, non-structural insulation system designed for commercial, industrial and residential applications. The Bayseal OCX system is comprised of an "A" component (aromatic diisocyanate) and a blended "B" component which includes polyols, fire retarding materials and catalysts. Bayseal OCX system has passed the International Code Council Acceptance Criteria 377 for spray-applied polyurethane foam insulation, Appendix X for use without the use of the prescribed ignition barrier. As with any product, use of Bayseal OCX foam-forming system must be tested (including, but not limited to, field testing) in advance by the user to determine suitability.

Covestro sold their spray polyurethane foam business to Accella in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.00960 g/cc0.00960 g/ccApparent; ASTM D1622
Viscosity 600 - 700 cP600 - 700 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 0.0434 MPa>= 6.29 psiASTM D1623
 
Thermal PropertiesMetricEnglishComments
Insulation R Value  3.9
@Thickness 25.4 mm
3.9
@Thickness 1.00 in
aged; ASTM C518
 13
@Thickness 88.9 mm
13
@Thickness 3.50 in
aged; ASTM C518

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Accella Bayseal® OC Polyurethane
BASF Basotect® G+ Foam
BASF Basotect TG Foam
BASF Basotect W Foam
BASF Basotect V3012 Foam

PCOVEST0228 / 202011

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.