MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow STRANDFOAM™ EA 1000 Polypropylene Foam  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Foamed

Material Notes: STRANDFOAM™ EA 1000 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibration dampening component in packaging, material transport, and automotive applications.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0400 g/cc0.00145 lb/in³DIN 53420
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 0.117 MPa17.0 psiat 25%, Horizontal; ASTM D3575, Suffix D
 0.138 MPa20.0 psiat 25%, Vertical; ASTM D3575, Suffix D
 0.317 MPa46.0 psiat 25%, Extruded; ASTM D3575, Suffix D
Compressive Modulus 0.00130 GPa0.189 ksiHorizontal; ASTM D3575, Suffix D
 0.00174 GPa0.252 ksiVertical; ASTM D3575, Suffix D
 0.00965 GPa1.40 ksiExtruded; ASTM D3575, Suffix D
Heat Distortion <= 1.0 %<= 1.0 %linear change at 180°F; ASTM D3575, Suffix S
 
Thermal PropertiesMetricEnglishComments
CTE, linear  57.6 µm/m-°C
@Temperature 20.0 °C
32.0 µin/in-°F
@Temperature 68.0 °F
Horizontal; ASTM D696
 72.0 µm/m-°C
@Temperature 20.0 °C
40.0 µin/in-°F
@Temperature 68.0 °F
Extrusion; ASTM D696
 73.8 µm/m-°C
@Temperature 20.0 °C
41.0 µin/in-°F
@Temperature 68.0 °F
Vertical; ASTM D696
Thermal Conductivity 0.0448 W/m-K0.310 BTU-in/hr-ft²-°FASTM D3575, Suffix V

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Neopolen® P 9270 0.11 g/cc Core density; Expanded Polypropylene (Europe)
Dow STRANDFOAM™ EA 1600 Polypropylene Foam
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Eurofoam Polycell PE 30 Polyethylene Foam
Armacell Ensolite™ MLC-Black PVC/NBR

PDOW1162 / 30380

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.