MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ashley Polymers Ashlene® 527LDMS Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: A very high impact Nylon 66 with Molybdenum disulfide designed to combine high impact with a reduced co-efficient of friction.

Data provided by the manufacturer

Key Words: Polyamide 66; Ashley Polymers, Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ASTM D792
Water Absorption 1.1 %1.1 %ASTM D570
Linear Mold Shrinkage 0.013 cm/cm0.013 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 113113ASTM D785
Tensile Strength, Ultimate 41.0 MPa5950 psiATSM D638
Elongation at Break 70 %70 %ASTM D638
Flexural Modulus 1.60 GPa232 ksiASTM D790
Izod Impact, Notched 9.08 J/cm17.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 254 °C489 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 213 °C415 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ashley Polymers Ashlene® 525LD-13G Nylon 66, 13% Glass Reinforced
Ashley Polymers Ashlene® 527LD Nylon 66
Ashley Polymers Ashlene® 527-25G Nylon 66, 25% Glass Reinforced
Ashley Polymers Ashlene® 525LD-33G Nylon 66, 33% Glass Reinforced
Ashley Polymers Ashlene® 527LDW Nylon 66

PNAB23 / 54470

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.