MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SunChemical Gwent F2071018D1 Transparent ITO Coated Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: This polyester film is produced by vacuum sputter deposition of indium tin oxide (ITO), this process provides excellent adhesion and uniform coating.
Used in components of touch screens and other position sensors, and electroluminescent (EL) lamps.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 175 microns6.89 milPolyester film thickness
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 80 ohm80 ohm
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.20 %
@Temperature 150 °C,
Time 1800 sec
0.20 %
@Temperature 302 °F,
Time 0.500 hour
heat stabilized
 
Optical PropertiesMetricEnglishComments
Haze 0.90 %0.90 %
Transmission, Visible 88 %88 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott Transparent ITO Conducting Oxide Coating
Indium Corp. Fine ITO Indium Tin Oxide
Indium Corp. Standard ITO Indium Tin Oxide
Reade Advanced Materials Indium-Tin Oxide (ITO) Powder (In2O3:SnO2)
Parker Chomerics WIN-SHIELD™ ITO (Coated) EMI Shielded Window

WGELZ9049 / 139362

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.