  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and processed according to good manufacturing practices, this resin is technically suitable for food contact end uses. This material complies with U.S. FDA Regulation 21 CFR 177.1520 c 3.2 (a) for food packaging applications. The regulation should be consulted for complete details.

Film properties below based on a film thickness of 40 µm. Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³
Thickness 40.0 microns1.57 mil
Melt Flow 1.0 g/10 min
@Load 2.16 kg
1.0 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 8.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 24.8 MPa3600 psiMolded property
Film Tensile Strength at Yield, MD 12.7 MPa1840 psi
Film Tensile Strength at Yield, TD 15.1 MPa2190 psi
Tensile Strength, Yield 15.1 MPa2190 psiMolded property
Film Elongation at Break, MD 670 %670 %
Film Elongation at Break, TD 780 %780 %
Elongation at Break 850 %850 %Molded value
Modulus of Elasticity 0.330 GPa47.9 ksiMolded Sample 2% Secant Modulus
Coefficient of Friction 0.600.60
Elmendorf Tear Strength MD 240 g240 g
Elmendorf Tear Strength TD 730 g730 g
Elmendorf Tear Strength, MD 6.00 g/micron152 g/mil
Elmendorf Tear Strength, TD 18.3 g/micron465 g/mil
Dart Drop 5.50 g/micron140 g/mil
Film Tensile Strength at Break, MD 39.6 MPa5740 psi
Film Tensile Strength at Break, TD 34.1 MPa4950 psi
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 106 °C223 °F
 
Optical PropertiesMetricEnglishComments
Haze 15 %15 %
Gloss 45 %45 %45°
 
Processing PropertiesMetricEnglishComments
Processing Temperature 232 °C450 °FFilm extrusion temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Borealis Borstar® FB2230 LLDPE for Film
Dow DOWLEX™ 2047G Linear Low Density Polyethylene
Dow DOWLEX™ 2517 Linear Low Density Polyethylene, Narrow MW Distribution
Dow DOWLEX™ 2027G Linear Low Density Polyethylene

PDW436 / 34505

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.