MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Bead Filled

Material Notes: Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Water Absorption 6.3 - 6.9 %6.3 - 6.9 %ISO 62
Moisture Absorption at Equilibrium 1.9 - 2.3 %1.9 - 2.3 %(23°C/50% R.H.); ISO 62
Viscosity Number 140 cm³/g1.40 dl/g
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/in
Melt Flow 93.8 g/10 min
@Load 5.00 kg,
Temperature 275 °C
93.8 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi50mm/min; ISO 527
Elongation at Yield 15 %15 %50mm/min; ISO 527
Modulus of Elasticity 3.00 GPa435 ksiISO 527
Flexural Strength 70.0 MPa10200 psiISO 178
Flexural Modulus 3.00 GPa435 ksiISO 178
Izod Impact, Notched (ISO) 8.50 kJ/m²4.04 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 9.00 J/cm²42.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²5.24 ft-lb/in²ISO 179/1eA
Tensile Creep Modulus, 1000 hours 2000 MPa
@Strain 0.5 %
290000 psi
@Strain 0.5 %
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 4.6
@Frequency 1e+6 Hz
4.6
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.070
@Frequency 1e+6 Hz
0.070
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 425 V425 VTest Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.40 J/g-°C0.335 BTU/lb-°F
Thermal Conductivity 0.340 W/m-K2.36 BTU-in/hr-ft²-°FDIN 53765
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 200 °C392 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °FInjection-molding/Extrusion
Mold Temperature 80.0 - 90.0 °C176 - 194 °FInjection-molding
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Dry)
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned)
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry)
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)

PBASF9304 / 85068

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.