MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mid-Mountain Materials HYTEX® 5000 High Carbon Industrial Textile (PAN)
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemistry and in differing configurations (cloth, tape, sleeving, rope etc.). Mid-Mountain can design hybrid materials by blending most any combination of yarns.

A family of textile products composed of heat-stabilized polyacrylonitrile fibers recommended for short term exposure to very high temperature.

Information provided by Mid-Mountain Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 371 °C700 °FContinuous
 482 °C900 °FShort Term
Maximum Service Temperature, Inert 2760 °C5000 °FContinuous
 3320 °C6000 °FShort Term
Decomposition Temperature 3650 °C6600 °F
 
Descriptive Properties
Abrasion ResistanceFair
Acid ResistanceExcellent
Alkali ResistanceGood
ColorBlack
CompositionPolyacrylonitrile 64% Carbon (PAN)
Solvent ResistanceExcellent
Sunlight & Aging ResistanceGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SGL Carbon Group PANOX® FM T320 EEA Oxidized Textile Fiber, Continuous Tow with 320k filaments, For carbon/carbon and spinning
DowAksa AKSACA™ A-38 3K Continuous Carbon Fiber
Sinotek Materials Packing Carbonized Fiber Braided
Solvay Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)

EMID00 / 5582

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.