MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NanoAmor 50% Regular Single Walled Carbon Nanotubes  (discontinued **)
Categories: Carbon

Material Notes: Applications
  • Additives in polymers
  • Catalysts
  • Electron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networks
  • Electromagnetic-wave absorption and shielding
  • Energy conversion
  • Lithium-battery anodes
  • Hydrogen storage
  • Nanotube composites (by filling or coating)
  • Nanoprobes for STM, AFM, and EFM tips, nanolithography, nanoelectrodes, drug delivery, sensors
  • Reinforcements in composites
  • Supercapacitor

Information provided by NanoAmor Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.0011 µm0.0011 µmAverage, from Raman Spectra
 0.00080 - 0.0016 µm0.00080 - 0.0016 µmfrom Raman Spectra
 0.0010 - 0.0020 µm0.0010 - 0.0020 µmfrom HRTEM
Specific Surface Area >= 400 m²/g>= 400 m²/g
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 10.0 - 1000 GPa1450 - 145000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0100 - 10000 ohm-cm0.0100 - 10000 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 50.0 - 200 W/m-K347 - 1390 BTU-in/hr-ft²-°F
 
Descriptive Properties
Colorblack
Length (um)5-15
Purity (vol% carbon nanotubes), min90
Purity (vol% single-walled nanotubes), min50

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrolytic Graphite, Low Temperature Isotropic (LTI)
NanoAmor 90% Regular Single Walled Carbon Nanotubes
NanoAmor 60% Regular Single Walled Carbon Nanotubes
NanoAmor 50% DWNT Double Walled Carbon Nanotubes
Graphite, Carbon, C

CNAN201 / 80003

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.