MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Bergamid™ B70 G30 BK Polyamide 6 (Nylon 6), DAM
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/cc±0.03; DIN 53479
Filler Content 30 %30 %Glass Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0010 - 0.0060 cm/cm
@Thickness 4.00 mm,
Temperature 23.0 °C
0.0010 - 0.0060 in/in
@Thickness 0.157 in,
Temperature 73.4 °F
Flow Bergmann Method; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 170 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
24700 psi
@Thickness 0.157 in,
Temperature 73.4 °F
5.0 mm/min; ISO 527
Elongation at Break 3.0 %
@Thickness 4.00 mm,
Temperature 23.0 °C
3.0 %
@Thickness 0.157 in,
Temperature 73.4 °F
5.0 mm/min; ISO 527
Tensile Modulus 9.50 GPa
@Thickness 4.00 mm,
Temperature 23.0 °C
1380 ksi
@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded; ISO 527-2/1
Charpy Impact Unnotched 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179
Charpy Impact, Notched 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 8.0 MPa 210 °C410 °FUnannealed; ISO 75-2/C
Flammability, UL94 HB
@Thickness 0.800 - 3.00 mm
HB
@Thickness 0.0315 - 0.118 in
ALL; Internal Method
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 280 °C464 - 536 °F
Mold Temperature 65.0 - 85.0 °C149 - 185 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
FeaturesGood Dimensional Stability
 Good Flow
 Good Stiffness
FormsPellets
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
Processing MethodInjection Molding
Regional AvailabilityEurope
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ B70 G30 BK Polyamide 6 (Nylon 6), Conditioned
Avient Bergamid™ A70 G15 HW TM-Z Polyamide 66 (Nylon 66)
DuPont Mobility and Materials Zytel® 70G30HSL BK039B PA66-GF30
Avient OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE)
Avient Bergamid™ A70 G35 UF SO Polyamide 66 (Nylon 66)

PH0POL1448 / 146017

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.