MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM A514 Steel, grade E, plate thickness ≤ 19 mm
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Low-alloy steel

The following are suggested consumables for arc welding processes: For 0.476 - 6.35 cm (3/16 - 2.5 in.) thicknesses - Manual Shielded Metal-Arc (AWS A5.5) Low Hydrogen Electrodes E11015, E11016, and E11018; Submerged Arc (AWS A5.23) F11x-Exxx; Gas Metal-Arc (AWS A5.28) ER110S; Flux Cored-Arc (AWS A5.29) E11xT. For 6.35 - 10.16 cm (2.5 - 4 in.) thicknesses - Manual Shielded Metal-Arc (AWS A5.5) Low Hydrogen Electrodes E11015, E11016, and E11018; Submerged Arc (AWS A5.23) F10x-Exxx; Gas Metal-Arc (AWS A5.28) ER100S; Flux Cored-Arc (AWS A5.29) E10xT.

Vanadium may be substituted for all or part of the titanium.

Key Words: UNS K21604, ASTM A 517 E
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³Typical of ASTM Steel
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 235 - 293
@Thickness 9.50 mm
235 - 293
@Thickness 0.374 in
for plates
Hardness, Knoop 289289Converted from Brinell
Hardness, Rockwell B 9898Converted from Brinell
Hardness, Rockwell C 2626Converted from Brinell
Hardness, Vickers 278278Converted from Brinell
Tensile Strength, Ultimate 760 - 895 MPa110000 - 130000 psi
Tensile Strength, Yield 690 MPa
@Strain 0.2 %
100000 psi
@Strain 0.2 %
Elongation at Break 18 %18 %in 50 mm
Bulk Modulus 160 GPa23200 ksiTypical for steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.0010 - 0.0050 %0.0010 - 0.0050 %
Carbon, C 0.12 - 0.20 %0.12 - 0.20 %
Chromium, Cr 1.4 - 2.0 %1.4 - 2.0 %
Iron, Fe 96 %96 %as balance
Manganese, Mn 0.40 - 0.70 %0.40 - 0.70 %
Molybdenum, Mo 0.40 - 0.60 %0.40 - 0.60 %
Phosphorus, P 0.035 %0.035 %
Silicon, Si 0.20 - 0.40 %0.20 - 0.40 %
Sulfur, S 0.040 %0.040 %
Titanium, Ti 0.010 - 0.10 %0.010 - 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A514 Steel, grade A, plate thickness ≤ 19 mm
ASTM A514 Steel, grade B, plate thickness ≤ 19 mm
ASTM A514 Steel, grade C, plate thickness ≤ 19 mm
ASTM A514 Steel, grade D, plate thickness ≤ 19 mm
ASTM A514 Steel, grade F, plate thickness ≤ 19 mm

MS514H / 13963

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.