MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayfill® 312 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System  (discontinued **)
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Information provided by Bayer Corporation, Polyurethanes Division

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0960 g/cc0.00347 lb/in³Molded density, ASTM D3574-A
Apparent Bulk Density 0.0720 g/cc0.00260 lb/in³Free-rise Density, Bayer test
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 0.270 MPa39.2 psiASTM D3574E
Elongation at Break 52 %52 %ASTM D3574E
Compressive Yield Strength 0.0440 MPa6.38 psi50% Compression, ASTM D3574-D
Tear Strength 0.300 kN/m1.71 pliSplit Tear Strength, ASTM D3574-F
Compression Set 54 %54 %Test C, ASTM D3574 Dry

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayfill® 310 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System
Covestro Bayfill® 361 Polyurethane Semi-Rigid Foam, Conventional Catalyst, Open Pour, MDI-based 2-Component Liquid System
Covestro Bayfill® 370 Polyurethane Semi-Rigid Foam, Polymeric Catalyst, Closed Pour, MDI-based 2-Component Liquid System
Covestro Bayfill® EA 4004 Polyurethane Energy-Absorbing Semi-Rigid Foam, Rigid Grade, MDI-based 2-Component Liquid System
Covestro Bayfill® 380 Polyurethane Semi-Rigid Foam, Polymeric Catalyst, Open Pour, MDI-based 2-Component Liquid System

PB2B31 / 26593

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.