MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chosun Refractories HACT-180 High Alumina Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.005886 - 0.008829 GPa
@Temperature 1000 °C,
Time 10800 sec
0.8537 - 1.281 ksi
@Temperature 1830 °F,
Time 3.00 hour
 0.005886 - 0.00981 GPa
@Temperature 1350 °C,
Time 10800 sec
0.8537 - 1.42 ksi
@Temperature 2460 °F,
Time 3.00 hour
 0.005886 - 0.00981 GPa
@Temperature 110 °C,
Time 86400 sec
0.8537 - 1.42 ksi
@Temperature 230 °F,
Time 24.0 hour
 0.007848 - 0.011772 GPa
@Temperature 1500 °C,
Time 10800 sec
1.138 - 1.7074 ksi
@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength  29.4 - 39.2 MPa
@Treatment Temp. 1000 °C,
Time 10800 sec
4270 - 5690 psi
@Treatment Temp. 1830 °F,
Time 3.00 hour
Cold Crushing Strength
 34.3 - 39.2 MPa
@Treatment Temp. 1350 °C,
Time 10800 sec
4980 - 5690 psi
@Treatment Temp. 2460 °F,
Time 3.00 hour
Cold Crushing Strength
 34.3 - 39.2 MPa
@Treatment Temp. 110 °C,
Time 86400 sec
4980 - 5690 psi
@Treatment Temp. 230 °F,
Time 24.0 hour
Cold Crushing Strength
 44.1 - 53.9 MPa
@Treatment Temp. 1500 °C,
Time 10800 sec
6400 - 7820 psi
@Treatment Temp. 2730 °F,
Time 3.00 hour
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  1.0817 W/m-K
@Temperature 260 °C
7.4951 BTU-in/hr-ft²-°F
@Temperature 500 °F
 1.1515 W/m-K
@Temperature 540 °C
7.9786 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 1.2097 W/m-K
@Temperature 800 °C
8.3816 BTU-in/hr-ft²-°F
@Temperature 1470 °F
Maximum Service Temperature, Air 1800 °C3270 °Flimited
Shrinkage  -0.200 %
@Temperature 1500 °C,
Time 10800 sec
-0.200 %
@Temperature 2730 °F,
Time 3.00 hour
 -0.100 %
@Temperature 1350 °C,
Time 10800 sec
-0.100 %
@Temperature 2460 °F,
Time 3.00 hour
 -0.0300 %
@Temperature 110 °C,
Time 86400 sec
-0.0300 %
@Temperature 230 °F,
Time 24.0 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 93 %93 %
 
Descriptive Properties
Installation MethodCasting
 Troweling
Material Required for Estimating (kg/m3)2,850
Water Required for Casting(%)8.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories HACT-155 High Alumina Castables
Chosun Refractories SAL85BR Special High Alumina brick
Chosun Refractories SAL90 Special High Alumina brick
Chosun Refractories HACT-150 High Alumina Castables
Chosun Refractories HACT-180G High Alumina Castables

CCHOS147 / 124091

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.