MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Essentium PCTG Additive Manufacturing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Glycol-Modified PCT (PCTG) Copolyester

Material Notes: Essentium Copolyester PCTG is a member of the copolyester family, chemically similar to PETG. Easy to use material with incredible surface finish and excellent impact resistance. Can be printed in open air and over a large temperature range. High temperatures produce glossy finish, low produce matte.

Definitions of axes used in property data table: XY is the print direction. ZX is the build direction. YX is the third orthogonal axis.

Information provided by Essentium Materials, LLC.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³Molded; ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 27.0 MPa3920 psiZX; ASTM D 638
 38.0 MPa5510 psiXY; ASTM D 638
 38.0 MPa5510 psiYX; ASTM D 638
 39.0 MPa5660 psiMolded; ASTM D 638
Tensile Modulus 1.426 GPa206.8 ksiZX; ASTM D 638
 1.507 GPa218.6 ksiYX; ASTM D 638
 1.67 GPa242 ksiXY; ASTM D 638
 1.748 GPa253.5 ksiMolded; ASTM D 638
Flexural Strength 53.0 MPa7690 psiZX; ASTM D 790
 60.0 MPa8700 psiYX; ASTM D 790
 68.0 MPa9860 psiMolded; ASTM D 790
 68.0 MPa9860 psiXY; ASTM D 790
Flexural Modulus 1.264 GPa183.3 ksiZX; ASTM D 790
 1.416 GPa205.4 ksiYX; ASTM D 790
 1.692 GPa245.4 ksiXY; ASTM D 790
 1.907 GPa276.6 ksiMolded; ASTM D 790
Izod Impact, Notched 0.250 J/cm0.468 ft-lb/inZX; ASTM D 256
 0.290 J/cm0.543 ft-lb/inYX; ASTM D 256
 1.09 J/cm2.04 ft-lb/inXY; ASTM D 256
 13.5 J/cm25.3 ft-lb/inMolded; ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Melting Point 202 °C396 °FMolded; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FMolded; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FMolded; ASTM D 648
Glass Transition Temp, Tg 76.0 °C169 °FASTM D 3418
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 - 260 °C410 - 500 °FExtrusion Temperature
Nozzle Temperature 275 °C527 °F
 
Descriptive Properties
Bed Temperature, °C23-60
Enclosure Temperature, °CRoom Temperature
Print SettingsInfill.: 100%; 30 mm/s, layer height: 0.3mm, extrusion multiplier: 1.0, nozzle diameter: 1.0 mm
Print Speed, mm/s30-70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Eastar DN004 PCTG Copolyester
Eastman Eastar DN102 PCTG Copolyester
CHT Group EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea
CHT Group EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea
Chosun Refractories PCT-AM-1 Monolithic Refractories for Ladle and Tundish

PESSEN903 / 220991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.