Daplen EE040AE is an elastomer modified polypropylene compound intended for injection molding. Daplen EE040AE is a material with excellent impact /stiffness ratio. Thanks to its low thermal expansion this material is suitable to mold parts requiring low change of dimensions over a broad temperature range. This product is optimized to give good surface aesthetics. Daplen EE040AE has been developed especially for bumpers and exterior trims. Information provided by the Manufacturer. |