MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID 66 GF 10 PA66, 10% glass fibre
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³
Viscosity Measurement 0.80 - 1.20.80 - 1.2
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/in
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/in
Melt Flow 3.0 g/10 min
@Load 0.325 kg,
Temperature 270 °C
3.0 g/10 min
@Load 0.716 lb,
Temperature 518 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psi
Elongation at Break 2.7 %2.7 %
Tensile Modulus 6.00 GPa870 ksi
Flexural Strength 170 MPa24700 psi
Flexural Modulus 5.50 GPa798 ksi
Charpy Impact Unnotched  3.00 J/cm²
@Temperature -20.0 °C
14.3 ft-lb/in²
@Temperature -4.00 °F
 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched  0.500 J/cm²
@Temperature -20.0 °C
2.38 ft-lb/in²
@Temperature -4.00 °F
 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °F
Vicat Softening Point 250 °C482 °FB
Flammability, UL94 HBHB
Glow Wire Test 650 °C1200 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned)
Overview of materials for Nylon 66, Unreinforced
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry)
Nylene® PA6/6 Glass Filled 5105 HS Nylon 6/6
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Dry)

PPLACO386 / 121010

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.