MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Assab Steels ASSAB XW-41 Cold Work Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Chrome-moly Steel; Tool Steel; Cold Work Steel

Material Notes: XW-41 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:
  • High wear resistance
  • High compressive strength
  • Good through-hardening properties
  • High stability in hardening
  • Good resistance to tempering-back.

XW-41 is used when cutting thicker, harder materials; when forming with tools subjected to bending stresses and where high impact loads are involved. XW-41 can be supplied in various finishes, including the hot-rolled, pre-machined and fine machined condition. It is also available in the form of hollow bar and rings.

AISI D2, W.-Nr. 1.2379

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.67 g/cc0.277 lb/in³
 7.61 g/cc
@Temperature 400 °C
0.275 lb/in³
@Temperature 752 °F
 7.64 g/cc
@Temperature 200 °C
0.276 lb/in³
@Temperature 392 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 41411020°C Austenitizing temperature, for tempering at 650°C
 44441050°C Austenitizing temperature, for tempering at 650°C
 55551020°C Austenitizing temperature, for tempering at 550°C
 57571050°C Austenitizing temperature, for tempering at 400°C
 59591020°C Austenitizing temperature, for tempering at 400°C
 60601050°C Austenitizing temperature, for tempering at 200°C
 6161At 980°C during hardening, soaking time 30 minutes
 62621050°C Austenitizing temperature, for tempering at 550°C
 6262Hardened and tempered.
 62.562.5At 980°C during hardening, soaking time 60 minutes
 63631020°C Austenitizing temperature, for tempering at 200°C
 64.2564.25At 1060°C during hardening, soaking time 30 minutes
 6565At 1020°C during hardening, soaking time 30 minutes
 65.565.5At 1020°C during hardening, soaking time 60 minutes
Modulus of Elasticity 193 GPa28000 ksi
 173 GPa
@Temperature 400 °C
25100 ksi
@Temperature 752 °F
Compressive Strength 1900 MPa276000 psiHRC 55 Rc0.2
 2200 MPa319000 psiHRC 62 Rc0.2.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.4 µm/m-°C
@Temperature 20.0 - 200 °C
6.89 µin/in-°F
@Temperature 68.0 - 392 °F
 13.4 µm/m-°C
@Temperature 20.0 - 400 °C
7.44 µin/in-°F
@Temperature 68.0 - 752 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity  20.0 W/m-K
@Temperature 20.0 °C
139 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 21.0 W/m-K
@Temperature 200 °C
146 BTU-in/hr-ft²-°F
@Temperature 392 °F
 23.0 W/m-K
@Temperature 400 °C
160 BTU-in/hr-ft²-°F
@Temperature 752 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.55 %1.55 %
Chromium, Cr 11.8 %11.8 %
Iron, Fe 84.35 %84.35 %
Manganese, Mn 0.40 %0.40 %
Molybdenum, Mo 0.80 %0.80 %
Silicon, Si 0.30 %0.30 %
Vanadium, V 0.80 %0.80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Assab Steels ASSAB XW-42 Cold Work Steel
Assab Steels ASSAB XW-5 Cold Work Steel
AISI Type A2 Tool Steel
AISI Type O1 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 425°C
AISI 1045 Steel, Quenched and Tempered to 390 HB

NASSAB04 / 15022

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.